Skip to product grid
-
- $4 NewNozzle≥0.2 mmDry before PrintingRequiredPrinting Temp.230-250 ℃Hotbed Temp.60-70 ℃ -
Hardness84-86 HDTensile Strength40-50 MPaElongation at Break12-16%Izod Impact Strength103 J/m -
Viscosity190-230 mPa.s(25℃)Hardness82-85 HDTensile Strength38-43 MPaElongation at Break16-22% -
Hardness84-86 HDTensile Strength40-50 MPaElongation at Break12-16%Izod Impact Strength103 J/m -
- $4 NewNozzle≥0.2 mmDry before PrintingRequiredPrinting Temp.230-250 ℃Hotbed Temp.60-70 ℃ -
Hardness82-84 HDTensile Strength35-45 MPaElongation at Break35-40%Izod Impact Strength212 J/m -
Hardness84-86 HDTensile Strength40-50 MPaElongation at Break12-16%Izod Impact Strength103 J/m